Abstract

This paper presents experimental data on the oxidation kinetics of a liquid 65 at % Pb + 35 at % Ge alloy in air. Lead metagermanate, PbGeO3, in a glassy state has been prepared by high-temperature oxidation of the melt at 1273 K. Interaction of molten PbGeO3 with crucible materials (SnO2, Au, Pd, and Pt) has been studied by the sessile drop method. Liquid lead germanate has been shown to be highly reactive with substrates from these materials. The heat capacity of the glassy lead metagermanate obtained has been determined by differential scanning calorimetry in the temperature range 300–800 K. In the range 330–630 K, the C p (T) data for glassy PbGeO3 can be represented using the Maier–Kelley equation. Above 630 K, there is a characteristic peak due to glass crystallization processes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.