Abstract
Mesophase-pitch-based graphite foams have attracted increasing attention because of their broad applications in thermal management, catalysis and so on. However, the common approach of using the high-pressure method for fabricating graphite foams is complex and risky. Herein, this research reports a simple and relatively safe technique for preparation of mesophase-pitch-based graphite foams, which is conducted under atmospheric pressure. Through foaming of mesophase pitch in the presence of epoxy resin at 700°C under atmospheric pressure and graphitization at 3000°C, graphite foam is fabricated. The obtained graphite foam is highly graphitic and has an open pore structure, the interlayer spacing of the (002) plane of which is about 0.3366 nm. Its density is 0.52 g/cm3 with a porosity of 73.5%. The properties of graphite foams can be tailored by modifying pitch particle sizes and foaming temperatures. With an increase in pitch particle size from <25 to 75–150 μm or in foaming temperature from 400 to 850°C, the pore sizes vary from 10–25 to 35–90 μm, and their bulk densities change from 0.50 to 1.11 g/cm3. Also, a foaming mechanism is proposed wherein the residue of epoxy resin can form a framework during heating, in which the pitch softens and decomposes, forming foam. This study suggests a relatively simple and safe method for production of graphite foams from mesophase pitch.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.