Abstract
High water absorption material was prepared by graft copolymerization of calcium lignin sulphonate with acrylic acid and acrylamide. Effect of process parameters on graft copolymerization and sample properties was investigated by means of the single-factor method, and the microstructure of fracture surface of the water absorbent resin was analyzed by SEM. The result shows that: when mass percents of acrylic, acrylamide, calcium lignin sulphonate, initiator and crosslinking agent are 65.5%, 19.5%, 15%, 0.09%, and 0.05%, respectively, and neutralization degree is 60% with 2h of initiation reaction time and 1.5h of crosslinking reaction time. The water absorption rate of material is up to 1010g/g, and 0.9wt% NaCl solution absorption rate is up to 110g/g.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.