This paper presented a novel process for production of furfural by hydrothermal degradation of corncob over biochar catalyst, in which it was prepared with the recycling degradation solution and lignocellulosic solid residues. The biochar catalyst was papered by lignocellulose residues and concentrated saccharide solution, and then impregnated in 0.5 mol/L sulphuric acid at room temperature for 24 h assisted by the ultrasonic vibration. In the system of recycling, 8.8 % lignocellulose residues and 100 % concentrated saccharide solution from corncob hydrolysis have been recycled. Hydrolysis of corncob was carried out at 180 °C for duration of 170 min over the biochar catalyst. The experimental results have shown that the furfural yield of up to 37.75 % and overall corncob conversion rate of 62.00 % could be achieved under optimum operating conditions for the catalysts preparation and the corncob hydrolysis. It is believed that the acid density of 4.27 mmol/g of biochar catalyst makes the SO3H groups cleave β-1,4 glycosidic linkages effectively and hydrolyze the cellulose and hemicellulose to water-soluble sugars, as well as to facilitate dehydration of xylose to give the product of furfural.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.