Abstract

Commercial acrylonitrile fibers of 1.2, 1.5, 3, 8 and 15 denier were separately treated in a 0.38 mol/l NH2OH methanolic solution at 80°C and then in a 0.1 mol/l NaOH aqueous solution at 30°C. The treatments were carried out by changing reaction periods to find the optimum conditions. The intrinsic adsorption rate of uranium from seawater with the amidoxime fibers was inversely proportional to fiber diameter, and the capacity was in the range of 120–350 mg per kg of dry fiber per day. The effective diffusivity of uranium in 1.5-denier amidoxime fiber immersed in seawater was 5 × 10–8 cm2/s. The strength of the fibers was not reduced by the NH2OH and NaOH treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.