Some semi-dry Flue Gas Desulfurization ash (SDFGDA) were taken from sinter gas of steel factory and been oxidized at experimental condition. Oxidized ash, granulated blast-furnace slag (GBFS) and steel slag were grinded and used to prepare cementing materials. Scanning electron microscope (SEM) was employed to identify the samples in order to investigate their hydration structure. The result shows that cementing materials have good hydration properties and mechanical properties, the initial and final setting time are qualified. It is recommended to control the Blaine fineness, mount of SDFGDA, ratio of GBFS/steel slag, mount of clinker to be 4500cm2/g, 19%, 1:4, 20%, respectively, when prepare eco-cement with those materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.