Abstract

BaTiO3 (BT) ceramics are prepared by spark plasma sintering (SPS) and conventional sintering. In conventional sintering, the density and grain size of the ceramics increase with sintering temperature. In SPS, ceramics with more than 97% relative densities can be obtained by sintering at 900 °C for 5 min in air atmosphere. Compared with conventional sintering, SPS suppresses grain growth in ceramics. The average grain size of the BT ceramics obtained by SPS and subsequent annealing at 1000 °C for 12 h is less than 1 µm. The ceramics exhibit a high relative dielectric constant of 6020. The field-induced displacement of the BT ceramics is larger than that of the ceramics sintered conventionally. The dynamic strain/field at 15 kV/cm was 540 pm/V.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.