Abstract

In this study, a 85/15 AN/MA copolymer (acrylonitrile – methylacrylate copolymer with feed ratio of 85/15 mol%) was synthesized by emulsion polymerization at 60 °C, and then the copolymer was used to produce hollow fiber (abbreviated as PAN hollow fiber )by melt spinning using a single screw extruder machine. The PAN hollow fiber was characterized by using Scanning Electron Microscope (SEM), Thermo-gravimetric Analysis (TGA) and Differential Scanning Calorimetry (DSC). The hollow fiber of melt-spinning PAN with high hollow rate of 51.1% has a homogeneous wall and regular section. The hollow fiber is potentially used as raw materials to fabricate heat preservation fabric for comfort clothing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.