Ultra-high temperature ceramic matrix composites (C/SiC–ZrB 2) are prepared by slurry and precursor infiltrations and pyrolysis method. C/SiC–ZrB 2 composites with ZrB 2 volume content from 10% to 24.6%, have balanced performance of fracture toughness (17.7–8.1 MPa m 1/2), flexural strength at room temperature (367–163 MPa) and at high temperature (strength retention 74% at 1800 °C and over 32% at 2000 °C), better oxidation and ablation resistance under oxyacetylene torch environment (recession rate 0.01 mm/s).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.