AbstractMechanical, thermal, and morphological properties of blends of high density polyethylene and poly(ethylene‐co‐1‐octene) (PEO) were evaluated. The blends were prepared in a single screw extruder at 230°C and 50 rpm with volume fraction of elastomer varying in the range from 0.05 to 0.8. Factors such as chemical similarity and melt viscosity favor the interdiffusion process of phases, resulting in better interfacial adhesion. A synergistic effect on the strength at break and elongation at break for a particular range of blend composition was observed. Blends with a volume fraction of PEO higher than 5% presented a super tough behavior at room temperature. Thermal analysis showed that there is a certain degree of interaction between high density polyethylene and PEO. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 81: 1991–1995, 2001

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.