Abstract

The formation of ligand-protected gold nanoclusters during size-selective syntheses is seemingly driven by the inherent properties of the protecting ligands, but a general description of the product formation has not been presented. This study uses diphosphine-protected Au clusters as a model system to examine i) control of metal-ligand complex distributions in methanol-chloroform solutions, ii) role of solution perturbations, e.g., oxidation, and iii) nanocluster formation through reduction of characterized complex distributions. By selectively reducing complexes and monitoring cluster formation with electrospray ionization mass spectrometry and UV-vis, data show the distribution of complexes can be controlled through ligand exchange, and the reduction of specific complexes produce characteristic ligated gold clusters based on ligand class. Specifically, 1,n-bis(diphenylphosphino)n-alkane ligands, L(n), where n = 1 through 6, are classified into two distinct sets. The classes represent ligands that either form mainly [AuL(n)(2)](+) (Class I, n = 1-3) or bridged [Au(2)L(n)(2)](2+) (Class II, n = 4-6) complexes after complete ligand exchange with AuClPPh(3). Selectively reducing gold-phosphine ligand complexes allows mapping of product formation, resulting collectively in a predictive tool for ligated gold cluster production by simply monitoring the initial complex distribution prior to reduction.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.