Abstract

AbstractCopper coated steel fibers reinforced LM13 aluminum alloy composites have been prepared using stir casting process. Experiments have been designed using response surface methodology (RSM) by varying wt % of reinforcement (0–10), stirrer speed (350 min−1–800 min−1) and pouring temperature (700 °C–800 °C). Microstructure and hardness of composites have been investigated. Analysis of variance, significance test and confirmation tests have been performed and regressions model has been developed to predict the hardness of composites. Response surface plots reveal that hardness of composites increases with increasing wt % of reinforcement and stirrer speed. The optimum stir cast process parameters for obtaining higher hardness are found to be the wt % of reinforcement of 8.2, pouring temperature of 748 °C and stirrer speed of 708 min−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.