Porous hydroxyapatite (HAp) monoliths were synthesized from gypsum mold waste with diammonium hydrogen phosphate solution by hydrothermal treatment at 50-190°C and their properties studied. Gypsum waste samples could be completely converted to HAp with 0.5 mol dm –3 (NH 4 ) 2 HPO 4 at 50°C in 15 days and 100°C in 2 days. This paper describes the effect of hydrothermal reaction conditions such as reaction temperature, time and concentration of (NH 4 ) 2 HPO 4 on the formation of new HAp monoliths and their porous properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.