Abstract

Pore size of Neosepta CMX (Tokuyama Soda, Japan), Selemion CMV (Asahi Glass, Japan) and heterogeneous HJC cation-exchange membrane (Hanguk Jungsoo, Korea) was characterized by chronopotentiometry in NH 4Cl and in other amine chloride solutions — simple homologous amine chloride, R–NH 3Cl, where R=CH 3, CH 2CH 3, (CH 2) 2CH 3, (CH 2) 3CH 3, (CH 2) 4CH 3, and (CH 2) 5CH 3. The chronopotentiometric curves obtained in the CMX and CMV membranes showed a steep inflection while diffusive in the heterogeneous HJC membrane. In all membranes, the inflections of chronopotentiometric curves became diffusive with the enlargement in molecular size of transporting ions. Assuming that the ion-exchange membrane consisted of conducting and non-conducting phases, Sand’s equation was modified in this study. Using the modified equation, the fraction of inert material contained in the membrane and the pore size were determined by comparing the theoretical and experimental transition times. The pore size of the membranes, determined by the chronopotentiometry method, correlated with membrane conductivity. It was considered that the diffusive inflection in the chronopotentiometric curve of the heterogeneous membrane was caused by the delay in the formation of the concentration gradient. This delay, in turn, was due to a high fraction of non-conducting region.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.