Abstract
AbstractThe structure, biodegradability, and morphological properties of composite materials composed of poly(butylene succinate adipate) (PBSA) and bamboo fiber (BF) were evaluated. Composites containing acrylic acid‐grafted PBSA (PBSA‐g‐AA/BF) exhibited noticeably enhanced compatibility between the two components. The dispersion of BF in the PBSA‐g‐AA matrix was highly homogeneous as a result of ester formation and the consequent creation of branched and crosslinked macromolecules between the carboxyl groups of PBSA‐g‐AA and hydroxyl groups in BF. In addition, the PBSA‐g‐AA/BF composite was more easily processed due to a lower melt viscosity. Each composite was subjected to biodegradation tests in an Acinetobacter baumannii compost. Morphological observations indicated severe disruption of film structure after 10–20 days of incubation, and both the PBSA and the PBSA‐g‐AA/BF composite films were eventually completely degraded. The PBSA‐g‐AA/BF films were more biodegradable than those made of PBSA and exhibited a lower molecular weight and intrinsic viscosity, implying a strong connection between these characteristics and biodegradability. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.