Abstract

Molybdenum oxide thin films are very appealing for gas sensing applications due to their tunable material characteristics. Particularly, the growing demand for developing hydrogen sensors has triggered the exploration of functional materials such as molybdenum oxides (MoOx). Strategies to enhance the performance of MoOx-based gas sensors include nanostructured growth accompanied by precise control of composition and crystallinity. These features can be delivered by using atomic layer deposition (ALD) processing of thin films, where precursor chemistry plays an important role. Herein, we report a new plasma-enhanced ALD process for molybdenum oxide employing the molybdenum precursor [Mo(NtBu)2(tBu2DAD)] (DAD = diazadienyl) and oxygen plasma. Analysis of the film thickness reveals typical ALD characteristics such as linearity and surface saturation with a growth rate of 0.75 Å/cycle in a broad temperature window between 100 and 240 °C. While the films are amorphous at 100 °C, crystalline β-MoO3 is obtained at 240 °C. Compositional analysis reveals nearly stoichiometric and pure MoO3 films with oxygen vacancies present at the surface. Subsequently, hydrogen gas sensitivity of the molybdenum oxide thin films is demonstrated in a laboratory-scale chemiresistive hydrogen sensor setup at an operation temperature of 120 °C. Sensitivities of up to 18% are achieved for the film deposited at 240 °C, showing a strong correlation between crystallinity, oxygen vacancies at the surface, and hydrogen gas sensitivity.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.