Abstract

Preparation conditions of tungsten powder by the decomposition of the scheelite concentrate in the medium of NaCl–Na2CO3, NaCl–Na2CO3–NaF, and NaCl–Na2CO3–Na3AlF6 salt melts and the reduction of formed sodium tungstate with aluminum at 1123–1273 K are investigated. It is established that the powder yield is ~93 wt % and purity of tungsten is 97%. Granulometric characteristics of powders are determined. It is shown that the specific surface of powders reaches 14.6 × 105 m–1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.