Two types of carbon nanotubes [single walled nanotubes (SWCNTs) and multi walled carbon nanotubes (MWCNTs)] are deposited on porous silicon by the drop casting technique. Upon exposure to test gas mixing ratio 3% NO2, the sensitivity response results show that the SWCNTs’ sensitivity reaches to 79.8%, where MWCNTs’ is 59.6%. The study shows that sensitivity response of the films increases with an increase in the operating temperature up to 200° and 150° for MWCNTs and SWCNTs. The response and recovery time is about 19 s and 54 s at 200° for MWCNTs, respectively, and 20 s and 56 s at 150° for SWCNTs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.