In this study, chitosan nanoparticles containing palmarosa essential oil (PEO-CNPs) were formed by ionotropic gelation, consisting of two parts: emulsion preparation followed by ionotropic gelation encapsulation with tripolyphosphate ions (TPP) as a crosslinker. The encapsulation method was optimized by varying three parameters, including chitosan concentration, initial oil loading in the emulsion and TPP concentration. The effects of these parameters on the encapsulation efficiency (EE) and loading capacity (LC) were analyzed. EE had an initial increase followed by a decrease in the range of three parameters. However, LC rose with varying initial oil content while it reduced with changing polymer and TPP concentration. The optimum experiment with the highest EE (10.0 g/L of chitosan, 5.0 g/L of TPP and 30.0 g/L PEO) was chosen to analyze the particle size using Dynamic Light Scanning method (DLS). With DLS measurement, the z-average diameter was 235.3 nm, and the particle size distribution was in the range of 100 – 500 nm.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Earth and Environmental Science
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.