Development of Mo composites based on the Mo-Si-B system has been demonstrated as a possible new route to achieving a high temperature Mobased material. In this new system, the silicide phases are replaced directly with silica or other silicate materials. These composites avoid the high ductile to brittle transition temperature observed for Mo-Si-B alloys by removing the Si that exists in solid solution in Mo at equilibrium with its silicides. A variety of compositions is tested for room temperature ductility and oxidation resistance. A system based upon Mo, Mo2B, and SrO·Al2O3·(SiO2)2 is shown to possess both ductility at 80 vol.% Mo and oxidation resistance at 60 vol.%. These composites can be produced using a powder processing approach and fired to greater than 95% theoretical density with a desirable microstructure of isolated boride and silicate phases within a ductile Mo matrix.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.