Abstract
This study examined retrieved UHMWPE tibial bearings made from a remelted highly crosslinked (HXL) UHMWPE to determine whether the material is chemically stable in vivo. Retrieved tibial components were measured for changes in ketone oxidation and crosslink density. Oxidation increased with in vivo duration, and a significant decrease in crosslink density with increased mean ketone oxidation index was observed. These results suggest that in vivo oxidation is causing material degradation. Furthermore, a subsurface whitened damage region was found below the articular surface of one bearing, indicating the possibility of a clinically relevant decrease in mechanical properties of this component. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 39-45, 2017.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of biomedical materials research. Part B, Applied biomaterials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.