Abstract

We have evaluated the thermal stability of Al2O3/LaAlO3/Si (001) stacks with atomic force microscopy, x-ray diffraction, transmission electron microscopy, and secondary ion mass spectrometry using a back side polishing approach. Crystallization of the amorphous LaAlO3 film was found to occur for rapid thermal anneals (RTA) above 935 °C for 20 s, in flowing N2. Penetration of Al and La into the underlying Si (001) is clearly observed for RTA at or above 950 °C for 20 s in flowing N2.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.