The rolling rate (r) dependence of textures was investigated in the Ti–26Nb–3Al (mol%) alloy to reveal the conditions required to form the {001}<110> recrystallization texture, which is a desirable orientation for the β-titanium shape memory alloy. {001}<110> was the dominant cold-rolling texture when r=90% and it was transferred to the recrystallization texture without forming {112}<110>, which is detrimental for the isotropic mechanical properties of the rolled sheet. A further increase in r resulted in the formation of {112}<110> in both rolling and recrystallization textures. Therefore, r should be controlled to form only the {001}<110> rolling texture, because the {112}<110> texture can overwhelm the {001}<110> texture during recrystallization.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.