Abstract

A novel and characteristic method is confirmed for enhancing the fibers/resin interfacial strength by growing MnO2 nanosheets on the woven carbon fiber (WCF) using the hydrothermal method for 1 h from 100 to 175 °C. An interesting finding is that both the density and length of MnO2 nanosheets are functions of the growth temperature. The optimal growth temperature is 125 °C, and the homogeneous and porous MnO2 has greatly improved the wettability between the WCF and the matrix and further results in an improvement of 16.3% and 30.2% in the flexural strength and tensile strength of the composite. And then tribological properties are further improved which can be verified by an obvious increment in dynamic fricition coefficient and a 38.7% reduction in wear rate.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.