Abstract
We propose here a deformation-induced diffusive phase transformation mechanism occurring during shearing of γ′ ordered phase in a γ/γ′ single crystalline CoNi-based superalloy. Shearing involved the creation and motion of a high density of planar imperfections. Through correlative electron microscopy and atom probe tomography, we captured a superlattice intrinsic stacking fault (SISF) and its associated moving leading partial dislocation (LPD). The structure and composition of these imperfections reveal characteristic chemical – structural contrast. The SISF locally exhibits a D019 ordered structure coherently embedded in the L12 γ′ and enriched in W and Co. Interestingly, the LPD is enriched with Cr and Co, while the adjoining planes ahead of the LPD are enriched with Al. Quantitative analysis of the three-dimensional compositional field in the vicinity of imperfections sheds light onto a new in-plane diffusion mechanism as the LPD moves on specific {111} planes upon application of stress at high temperature.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.