Abstract

To investigate the range of “coupled” eutectic growth in Al-Co alloys from 1 to 4 wt% Co and Al-Ni alloys from 5 to 10 wt% Ni directional solidification, using rates from 0.8×10−2 cm/sec to 10.6×10−2 cm/sec, was employed. Both alloy systems exhibited coupled zones skewed towards the hypereutectic compositions. Fully eutectic structures were obtained in the ranges Al-1 wt% Co to Al-3 wt% Co and Al-5.7 wt% Ni to Al-9.2 wt% Ni.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.