Abstract
In this study, indentation and fracture of compliant low-dielectric constant (low-k) films on silicon substrates was investigated by means of finite element (FE) modelling. Cohesive zone damage models were employed for fracture simulation and damage constitutive parameters and plastic yield stress of organosilicate glass 2.4 (OSG 2.4) low-k films coated on silicon substrates were obtained by correlating the force-displacement and crack growth response with experiments. The model lends itself to characterization of brittle films where the value of the Young's modulus, the maximum cohesive strength, the critical cohesive energy release rate and plastic yield stress of the low-k films can be extracted only by conducting cube corner indentation experiments and employing the finite element model.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.