Taking the automobile control arm as the research object, using MAGMASOFT, to simulate the squeeze casting process, the position of the shrinkage cavity and shrinkage defects in the casting process is accurately predicted. The results show that there exist shrinkage defects in the end and middle of the upper arm. The top of the upper arm is partially squeezed, and partial squeeze pressure is 130 MPa, the hotspot is eliminated. In the middle of the upper arm, the cooling line is added, so the control arm is whole to meet the order of solidification principle, and shrinkage defects are eliminated.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.