To pertinently balance growth kinetics, solidification thermodynamics and dendrite expitaxy of multicomponent nickel-based single-crystal supralloy during laser processing, effect of thermometallurgy determinant factors, including laser power, welding speed and welding configuration, on solidification behavior, such as nonequilibrium solidification temperature range, and dendrite growth, such as dendrite trunk spacing, are progressively advanced to forestall solidification cracking phenomena. Symmetric developments of dendrite trunk spacing and solidification temperature range alongside solid/liquid interface are crystallographically driven by useful (001)/[100] welding configuration to auspiciously bring about crack-insusceptible and well-oriented dendrite growth. Dissimilarly, unsymmetrical developments of dendrite trunk spacing and solidification temperature range alongside solid/liquid interface are crystallographically driven by (001)/[110] welding configuration to insidiously favor crack-unresistant and disoriented dendrite growth. Higher heat input thermodynamically and kinetically boosts wide solidification temperature range, appalling stray grain growth with excess of solute ahead of dendrite tip and large size of crack-unresistant region to thermometallurgically disintegrate epitaxial growth for untoward solidification cracking, and therefore should be strictly withstood. Although geometry of symmetrical weld pool both sides is the same in infelicitous (001)/[110] welding configuration, [100] region of dendrite growth is more liable to ruinous stray grain growth and extensive solidification temperature range than [010] region of dendrite growth to complicate dendrite growth and exacerbate weld integrity. The determinant mechanism of crystallography-aided amelioration of solidification cracking resistance as result of kinetics-and thermodynamics-driven dendrite growth is propitiously proposed. Furthermore, the credible and understandable theoretical predictions are in conformity with the experiment results.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.