Abstract

The high whiteness tourmaline composite powder was prepared with powder coating method in which TiO2 as the coating agent and the stearic acid as the coupling agent. The powder coating method system theoretical research was improved to aim at resolving the tourmaline’s limited applications in environmental health field due to the darker color. Theory and test results show that when the tourmaline and the coating agent mass ratio of about 2:1, the best results by scanning electron microscopy indicating that the tourmaline composite powder particle size prepared of this ratio is uniform with the composite powder whiteness of 74.5% which is 23.5% higher than building whiteness of the direct coating agent for mechanical mixing with tourmaline powder. After the composite powder was used to prepare the coating, the results show that the whiteness is 87.1% after formatting coating and negative ions incremental release over the 800 ions/cm3 when the content of tourmaline is 11%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.