Abstract

The authors state that an analysis of the mechanical properties and wear resistance of the experimental steels makes it possible to recommend them for use in various branches of machine building. In petroleum machine building this steel may be recommended for the production of parts of the drive chains of drilling units in place of 30KhN3A, 12KhN3A, and 50KhFA steels. This is also a basis for expecting a definite effect from the use of such steels in the mining industry and in construction. The paper reports on studies of experimental steels based on the premise that an analysis of the designs and operating conditions of rapidly wearing parts of well-drilling equipment has shown that the primary reason for their unsatisfactory life span is the low mechanical properties of the steels used.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.