Telechelic oligo(ether–ketone)s containing two trimethylsiloxy end groups and one methyl group per repeating unit were prepared by polycondensation of 4-fluoro-2′-methyl-4′-(trimethylsiloxy)benzophenone. The telechelic character was achieved by cocondensation of a small amount of silylated bisphenol-P. The end groups of the silylated oligo(ether–ketone)s were acetylated by means of acetyl chloride. On the basis of 1H-NMR end group analyses two samples of α,ω-bis(acetoxy) oligo(ether–ketone)s with DP = 14 and DP ∼ 28 were obtained. These oligo(ether-ketone)s and a 70 or 140 fold molar amount of silylated 3,5-bis(acetoxy)benzoic acid were polycondensed at 270°C in bulk. The resulting A–B–A triblock copolymers were fractionated by dissolution in tetrahydrofuran. In three out of four experiments a small fraction of precipitated material rich in oligo(ether–ketone) was isolated. The purified triblock copolymers were characterized by inherent viscosities and NMR spectra. For those samples containing the long oligo(ether–ketone) block a low degree of crystallinity was observed after annealing. Four additional polycondensations were conducted with an initial reaction temperature of 290°C. In this way a completely soluble and amorphous triblock copolymer was obtained. © 1998 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 36: 31–38, 1998
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science Part A: Polymer Chemistry
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.