The properties of a reinforced gel with partially hydrolyzed polyacrylamide (HPAM) as the main agent, water-soluble phenolic resin (WSPR) as the crosslinker, and nano-SiO2 as the stabilizer were evaluated in terms of gelation time, gel strength and thermal stability under the conditions of 110 °C and 12.124 g/L salinity in water. The results showed that the gelation time of the gel with high strength was adjustable from 3 to 23 h, remaining stable for more than 180 days under stratigraphic conditions, although with a certain degree of early dehydration in the gel. Cryo-scanning electron microscopy (cryo-SEM) and dynamic light scattering (DLS) analysis revealed that nano-SiO2 improves the dispersion of the polymer in water, resulting in a more homogeneous structure of the formed gel and thus improving the strength of the gels. In addition, rheological tests and cryo-SEM showed that the interaction between nano-SiO2 and the polymer could inhibit the degradation of polymer to a certain extent and improve the thermal stability of the gel. However, the oxidative degradation of the gel is still the main cause of early dehydration of water-soluble phenolic resin gel, and the addition of a small amount of hydroquinone to the gelants can significantly improve the antioxidative degradation properties of phenolic resin gel.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.