NaK alloy in contact with 15-crown-5 hexane solution became potassium sodide K +(15-crown-5) 2Na −. After the evaporation of hexane the crystalline solid product was analyzed by X-ray diffraction and the lattice parameters were calculated. The potassium sodide thus obtained could be easily dissolved in tetrahydrofuran. A deep blue solution containing sodium anions and complexed potassium cations was formed with a very low concentration of solvated electrons, i.e. of the order of 10 −7 M. Potassium anions were not detected in this case. A new crystalline potassium sodide K +(DCH-24-crown-8) 2Na − was obtained using NaK alloy and dicyclohexano-24-crown-8 hexane solution.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.