Abstract

Nanoindentation technique was used to investigate the mechanical properties of polypropylene/multi-wall carbon nanotubes (MWCNT) nanocomposite fibers. The hardness and elastic modulus of the nanocomposite fibers were evaluated as a function of MWCNT concentration. It was found that incorporation of MWCNT enhanced the hardness and elastic modulus of the fibers. The elastic modulus data calculated from indentation load–displacement experiments were comparable with those obtained from tensile tests. DSC results also confirmed the increase in crystallinity of the polypropylene fibers due to the addition of MWCNT. The studies indicated that nanoindentation was a simple but efficient test method for evaluating the mechanical properties of nanocomposite fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.