Abstract

Experimental and theoretical studies were carried out to clarify shape control of alumina inclusions during calcium double treatment in a line pipe steel for sour service. Calcium (Ca) double addition method were experimented by 280 t-scale commercial plant.In this method, Ca powder was firstly injected for shape control of alumina inclusions by flux injection process (FI), and was secondly added for shape control of MnS to CaS in tundish of continuous casting machine after eliminating the first step Ca by RH degasser.The degree of shape control of alumina inclusions of this method was increased compared with that of the conventional Ca treatment by FI or tundish addition, and approaches to the equilibrium condition among Ca-CaO-Al2O3 system. To explain the shape control rate of alumina inclusions, the non-reacted core model fitted by the laboratory scale experimental results was applied for this experimental data. The calculated values from this model in the Ca double addition method agreed well with the observed ones.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.