Abstract
Cr2B, CrB and CrB2 ceramics were prepared by hot-pressing of the powders synthesized via the solid state reactions between metallic chromium and amorphous boron powders. Cr2B ceramics were prepared in the temperature range of 1200-1600°C. CrB ceramics were prepared in the temperature range of 1500-1900°C. CrB2 ceramics were prepared in the temperature range of 1400-1900°C. It was observed that CrB2 possesses more excellent sinterability than Cr2B amd CrB. The hardness of CrB2 ceramics increased with the sintering temperature up to 1700°C and then decreased owing to grain coarsening. As an excellent etching method of CrB2 ceramics, the electrolytic etching method was developed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society of Powder and Powder Metallurgy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.