Abstract

The Fe-Al-C permanent-magnet alloy —the MT Magnet steel— is well adapted to a country like Japan limited in natural resources. As this alloy owns coercive force of more than 200 Oe, it can be applied to such equipments as watt-hour meter, hysteresis or small DC motors in place of Co or Cr magnet steel. The results of fundamental researches on MT magnet were already reported in the author’s previous papers. Accordingly, this report covers a part of later experiments conducted in the course of industrialization. In melting procedure, it is necessary to take care of segregation and oxidation of the alloying Al. In view of yielding rate of magnetic properties and heat treatment, it was discovered that the most appropriate composition of MT magnet was within the region of 8.15±0.25%Al and 1.99±0.03%C. Addition of Si is harmful for magnetic properties and Si must be kept below 0.20%. Casting has been made in green sand. The design of the pattern, the “as-cast” tolerance and the defects in casting were reexamined in the light of daily practices.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.