Abstract
A modulated-temperature differential scanning calorimetry (M-TDSC) method for the analysis of interphases in multi-component polymer materials has been developed further. As examples, interphases in a polybutadiene-natural rubber (50:50 by mass) blend, a poly(methyl methacrylate)-poly(vinyl acetate) (50:50 by mass) structured latex film, a polyepichlorohydrinpoly(vinyl acetate) bilayer film, and polystyrene-polyurethane (40:60 by mass) and poly(ethyl methacrylate)-polyurethane (60:40 by mass) interpenetrating polymer networks were investigated. The mass fraction of interphase and its composition can be calculated quantitatively. These interphases do not exhibit clear separate glass transition temperatures, but occur continually between the glass transition temperatures of the constituent polymers.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.