Abstract

Effect of spray rate on structural, optical and electrical properties of spray pyrolysed Cu2ZnSnS4 (CZTS) thin films was investigated. We deposited films by varying spray rate from 2 ml/min to 10 ml/min in steps of 2 ml/min. For very low and high spray rates presence of secondary phases could be observed while for the films prepared at a spray rate of 6 ml/min were devoid of secondary phases. As spray rate increases band gap decreased. Samples prepared at 6 ml/min had optimum band gap of 1.5 eV. All the samples were observed to be p-type. Resistivity values increased steadily up to 6 ml/min and then slightly decreased. From the present work, CZTS films prepared at a spray rate of 6 ml/min is found to be ideal for absorber layer in solar cell.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.