Mn-kaolinite was hydrothermally synthesized, for the first time, using silicic acid, Mn-carbonate and aluminum nitrate mixed with aqueous solutions of KOH at 100–200 °C for 24–96 h. Without the addition of Mn-carbonate to silicic acid and aluminum nitrate mixture, no crystalline material could be synthesized by hydrothermal treatment up to 200 °C for 6 days. However, by the addition of Mn-carbonate to the above precursors, Mn-kaolinite was synthesized at both 100 and 200 °C for 1 or 2 days, indicating that Mn played an important role in the formation of kaolinite. At a reaction temperature of 100 °C, the Mn-kaolinite peaks became sharper with increasing reaction duration, as expected.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.