Abstract

The CdWO4 compound was prepared from CdO and WO3 mixtures by high energy ball milling method and its microwave dielectric properties have been investigated. After milling 30 h, pure and well-crystallized CdWO4 powders with an average grain size of 230 nm were obtained at 125°C. The CdWO4 ceramics sintered at 950–1100°C have monoclinic structure belong to the space group P2/c(13), and when sintered at 1025°C, the ceramics exhibited good dielectric constant (ϵr) of ∼ 12.81, Q×f of ∼27000 GHz and τf of ∼−19.3 ppm/°C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.