Abstract
The microstructure evolution of a FeNiCr alloy oxidized at 600 °C by simultaneously applying stress via high temperature nanoindentation is reported. Analysis using transmission electron microscopy shows that a sharp crack was induced beneath the indentation area under the stress-oxidation coupling condition. Nanotwins beneath the indentation area were also observed, which acted as a barrier that ceased the crack propagation beneath the indenter by altering the path of the crack. Results reveal a transformation from inter-granular crack propagation along the oxide grain boundaries to intra-granular crack propagation through the nanotwin structure with a zig-zag pattern.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.