In this study, modification of aluminium silicon eutectic alloy by grain modifier, strontium was investigated on conventional and slope cast A356 alloy. A356 alloy with addition of 0 to 0.97 wt.% Sr was prepared by conventional and slope casting in melting furnace. The molten metal of A356 alloy was casted into steel mould. Microstructure was observed using SEM. Phase analysis was done using XRD. Microhardness was conducted using Vicker microhardness. Microstructure of conventional cast displayed dendritic structure whereas slope cast displayed globular structure. Addition of Sr refined eutectic structure in both conventional and slope cast alloy. Phase analysis revealed the presence of Al2Sr phase in conventional cast Al-6Si-0.97Sr. Microhardness of the conventional cast alloy decreased with increasing of Sr up to 0.97 wt.%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.