Abstract

The Si 3 N 4 coating and Si 3 N 4 coating with Si 3 N 4 whiskers as reinforcement (Si 3 N 4w -Si 3 N 4 ) were prepared by chemical vapor deposition (CVD) on two-dimensional silicon nitride fiber reinforced silicon nitride ceramic matrix composites (2D Si 3 N 4f /Si 3 N 4 composites). The effects of process parameters of as-prepared coating including the preparation temperature and volume fraction of Si 3 N 4w on the microstructure and mechanical properties of the composites were investigated. Compared with Si 3 N 4 coating, Si 3 N 4w -Si 3 N 4 coating shows more significant effect on the strength and toughness of the composites, and both strengthening and toughening mechanism were analyzed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.