Abstract

Silica-based ceramic cores play key roles in the casting of aeroengine blades, but they are highly limited by the poor high-temperature mechanical property. Here, fused mullite (FM) and sintered mullite (SM) powders were modified in silica-based ceramic cores, and the microstructure evolution and crystallization kinetics of ceramic cores depending on mullite types were studied. The ceramic cores with FM showed a dense microstructure and superior mechanical properties compared to those with SM. The ceramic cores with 10 wt.% of FM showed a crystallization activation energy of 1119.5 kJ/mol and a crystallization exponent of 1.74, and the values of 938.4 kJ/mol and 1.86 as SM were employed; the decreased crystallization activation energy and the elevated crystallization exponent by SM suggested that the excess impurities of alkali oxides and alkaline-earth oxides significantly promoted the crystallization of cristobalite. Even though the ceramic cores with mullite powders decreased slightly in the room-temperature mechanical property, their high-temperature flexure strength and creep deformation resistance were enhanced. The ceramic cores with 10 wt.% of FM showed excellent comprehensive performance, with linear shrinkage of 0.69%, room-temperature strength of 18.9 MPa, and high-temperature strength of 15.5 MPa, which satisfied the demands for hollow-blade casting.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.