Nanoporous gold was fabricated by dealloying a rolled Au0.3Ag0.7 sheet and the effects of thermal and acid treatments on the porous structure and (111) texture were investigated. Both of the coarsening treatments increased the pore and ligament sizes to approximately 500 nm, whereas the resulting porous structure was very different between the two treatments. After the thermal treatment, the (111) plane was highly oriented in a specific direction; however, the change in the (111) texture after the acid treatment was less pronounced than that after the thermal treatment. There may be difference in migration routes of Au atoms between the two treatments.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.