Abstract

A fine-grained yttria stabilized tetragonal zirconia exhibits an optimum superplastic elongation to failure of ∼ 700% at 1823 K and a strain rate of 8.3 × 10 −5s −1. A detailed microstructural investigation of the superplastically deformed specimens reveals the occurrence of extensive concurrent grain growth and internal cavitation. An expression is developed to characterize the extent of deformation enhanced concurrent grain growth, as influenced by experimental factors such as true strain, strain rate and temperature. The variation in the level of concurrent cavitation with strain rate conforms closely to the variation in elongation to failure with strain rate. It is demonstrated that the tendency towards cavity interlinkage in a direction perpendicular to the tensile axis is an important factor influencing the total elongation to failure obtained in superplastic materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.