Abstract

Ni-16Mo and ODS alloys were fabricated by the powder metallurgical processes, and their microstructures and tensile properties were investigated. Ni-16Mo-7Cr and Ni-16Mo-7Cr-0.3Ti-0.35Y2O3 (in wt.%) alloys were prepared by mechanical alloying, uniaxial hot pressing, and heat treatment processes. Microstructural observations of these alloys revealed that the Ti and Y2O3 additions to a Ni-16Mo alloy were significantly effective to refine the grain size and form nano-sized Y-Ti-O oxide particles. Consequently, the tensile strengths at room temperature and 700°C were considerably enhanced. This improvement of tensile properties can be mainly attributed to the formation of nano-sized oxide particles, as well as the refined grain size. It is thus concluded that Ni-16Mo alloy with Ti and Y2O3 additions would be very effective in improving the mechanical properties especially at elevated temperatures.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.