Abstract

Microstructural evolution and plastic flow characteristics of a Ni-based superalloy were investigated using a simulative model that couples the basic metallurgical principle of dynamic recrystallization (DRX) with the two-dimensional (2D) cellular automaton (CA). Variation of dislocation density with local strain of deformation is considered for accurate determination of the microstructural evolution during DRX. The grain topography, the grain size and the recrystallized fraction can be well predicted by using the developed CA model, which enables to the establishment of the relationship between the flow stress, dislocation density, recrystallized fraction volume, recrystallized grain size and the thermomechanical parameters.

Highlights

  • The mechanical properties of a metallic component such as high-temperature alloy are largely depended on their chemical composition and microstructures, resulting from processing and heat treatment history in industrial production

  • Where the two terms represent a competition between storage of mobile dislocations and dynamic annihilation of dislocations, k1 represents work hardening, k2 is the softening parameter that represents the recovery of dislocation. k1 and k2 in Eq (3) can be evaluated from the measured flow stress and can be expressed as functions of temperature and strain rate

  • In the cellular automaton (CA) model for recrystallization, the transformation of a cell from the unrecrystallized state to the recrystallized state can be initiated when the following conditions are fulfilled simultaneously: (1) The driving force is positive; (2) The cell is at the grain boundary; at least one cell in the von Neumann neighborhood is already in the recrystallized state; (3) The recrystallized fraction variable is equal to 1; (4) The computer-generated random number is less than the transformation probability P, which is defined as P = i/4, where i is the number of neighboring cells, which have the same orientation in the von Neumann neighborhood

Read more

Summary

Introduction

The mechanical properties of a metallic component such as high-temperature alloy are largely depended on their chemical composition and microstructures, resulting from processing and heat treatment history in industrial production. There are many cases of successful application of CA in modeling microstructural evolution In these studies, Ding et al [5], Raabe [6], Kugler and Turk [7], Xiao and Zheng [8] and Jin and Cui [9] contributed greatly to the development of the CA method for the simulation of DRX from the aspects of optimization algorithm, grain morphology change and. In order to deeply understand DRX mechanism and to predict and control the microstructure evolution during DRX for IN718, there is a need to develop new model to simulate the grain refinement during hot working from mesoscale aspect. By using the developed model, a wide range of deformation temperature and strain rate over DRX were examined to investigate the quantitative and topographic prediction of the microstructural evolution during hot working for IN718 superalloy. The appropriate hot working parameters for IN718 were recommended based on the CA simulations

Experiment materials and procedures
Flow characteristics
Mechanism of CA simulation of DRX
Modeling of dislocation evolution
Modeling of nucleation and grain growth
Consideration of grain geometry of real deformation
Implementation of recrystallization in CA model
Determination of k1 and k2
Parameter categories
Reverse method of determination of nucleation parameter
Simulation results and discussion
Findings
Conclusions
Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.